Marcosz schreef op 8 april 2019 16:05:
had nog niet gezien dat dit werd aangevuld op de site van Nyrstar:
January 2019
- 28kt of feed treated in the TSL furnace
- Feed to the furnace consisted of 44% concentrates and 56% residues
- 20.7kt of slag and 10.4kt of acid were produced by the TSL furnace
February 2019
- 34.4kt of feed treated in the TSL furnace
- Feed to the furnace consisted of 39% concentrates and 61% residues
- 27.2kt of slag and 11.4kt of acid were produced by the TSL furnace